Pitting Initiated by MnO·Cr2O3–MnS and MnS Inclusions in a Si‐/Mn‐Killed Stainless Steel.

التفاصيل البيبلوغرافية
العنوان: Pitting Initiated by MnO·Cr2O3–MnS and MnS Inclusions in a Si‐/Mn‐Killed Stainless Steel.
المؤلفون: Liu, Zhen, Ren, Qiang, Zhang, Lifeng
المصدر: Steel Research International; Sep2024, Vol. 95 Issue 9, p1-13, 13p
مصطلحات موضوعية: STAINLESS steel corrosion, STAINLESS steel, MANGANOUS sulfide, SULFUR, STEEL
مستخلص: Two types of inclusions in the stainless steels are detected: MnO·Cr2O3–MnS dual‐phase ones and pure MnS ones. The increase of sulfur content can inhibit the formation of MnO–Cr2O3–MnS inclusions and reduce the harm of MnO·Cr2O3–MnS inclusions on the pitting corrosion of stainless steels. When the sulfur content increases from 26 to 70 ppm, the average pitting potential increases from 0.34 to 0.4 VSCE due to the decrease in the number density of MnO–Cr2O3–MnS inclusions. A Cr‐depletion zone exists in the steel matrix around MnO–Cr2O3–MnS inclusions. The size of pits induced by MnO·Cr2O3–MnS inclusions is larger, which poses a more serious threat to the pitting resistance of stainless steels. [ABSTRACT FROM AUTHOR]
Copyright of Steel Research International is the property of Wiley-Blackwell and its content may not be copied or emailed to multiple sites or posted to a listserv without the copyright holder's express written permission. However, users may print, download, or email articles for individual use. This abstract may be abridged. No warranty is given about the accuracy of the copy. Users should refer to the original published version of the material for the full abstract. (Copyright applies to all Abstracts.)
قاعدة البيانات: Complementary Index
الوصف
تدمد:16113683
DOI:10.1002/srin.202400144