Optical and microstructural characterization of Er3+ doped epitaxial cerium oxide on silicon.

التفاصيل البيبلوغرافية
العنوان: Optical and microstructural characterization of Er3+ doped epitaxial cerium oxide on silicon.
المؤلفون: Grant, Gregory D., Zhang, Jiefei, Masiulionis, Ignas, Chattaraj, Swarnabha, Sautter, Kathryn E., Sullivan, Sean E., Chebrolu, Rishi, Liu, Yuzi, Martins, Jessica B., Niklas, Jens, Dibos, Alan M., Kewalramani, Sumit, Freeland, John W., Wen, Jianguo, Poluektov, Oleg G., Heremans, F. Joseph, Awschalom, David D., Guha, Supratik
المصدر: APL Materials; Feb2024, Vol. 12 Issue 2, p1-9, 9p
مصطلحات موضوعية: CERIUM oxides, SILICON oxide, MOLECULAR beam epitaxy, ELECTRON spin, SILICON films, EPITAXY
مستخلص: Rare-earth ion dopants in solid-state hosts are ideal candidates for quantum communication technologies, such as quantum memories, due to the intrinsic spin–photon interface of the rare-earth ion combined with the integration methods available in the solid state. Erbium-doped cerium oxide (Er:CeO2) is a particularly promising host material platform for such a quantum memory, as it combines the telecom-wavelength (∼ 1.5 μ m) 4f–4f transition of erbium, a predicted long electron spin coherence time when embedded in CeO2, and a small lattice mismatch with silicon. In this work, we report on the epitaxial growth of Er:CeO2 thin films on silicon using molecular beam epitaxy, with controlled erbium concentration between 2 and 130 parts per million (ppm). We carry out a detailed microstructural study to verify the CeO2 host structure and characterize the spin and optical properties of the embedded Er3+ ions as a function of doping density. In as-grown Er:CeO2 in the 2–3 ppm regime, we identify an EPR linewidth of 245(1) MHz, an optical inhomogeneous linewidth of 9.5(2) GHz, an optical excited state lifetime of 3.5(1) ms, and a spectral diffusion-limited homogeneous linewidth as narrow as 4.8(3) MHz. We test the annealing of Er:CeO2 films up to 900 °C, which yields narrowing of the inhomogeneous linewidth by 20% and extension of the excited state lifetime by 40%. [ABSTRACT FROM AUTHOR]
Copyright of APL Materials is the property of American Institute of Physics and its content may not be copied or emailed to multiple sites or posted to a listserv without the copyright holder's express written permission. However, users may print, download, or email articles for individual use. This abstract may be abridged. No warranty is given about the accuracy of the copy. Users should refer to the original published version of the material for the full abstract. (Copyright applies to all Abstracts.)