العنوان: Preparation and properties of emulsifier-/solvent-free slightly crosslinked waterborne polyurethane-acrylic hybrid emulsions for footwear adhesives (III)–effect of trimethylol propane (TMP)/ethylene diamine (EDA) content
المؤلفون: Cha-Cheol Park, Joo-Yeong Che, Jae-Hwan Chun, Young-Hee Lee, Jungmi Cheon, Han-Do Kim
المصدر: Journal of Adhesion Science and Technology. 31:1872-1887
بيانات النشر: Informa UK Limited, 2017.
سنة النشر: 2017
مصطلحات موضوعية: Acrylate, Materials science, 02 engineering and technology, Surfaces and Interfaces, General Chemistry, Dynamic mechanical analysis, 010402 general chemistry, 021001 nanoscience & nanotechnology, 01 natural sciences, 0104 chemical sciences, Surfaces, Coatings and Films, Viscosity, chemistry.chemical_compound, Chemical engineering, chemistry, Mechanics of Materials, Propane, Polymer chemistry, Ultimate tensile strength, Emulsion, Materials Chemistry, Adhesive, 0210 nano-technology, Polyurethane
الوصف: Stable emulsions of emulsifier-/solvent-free slightly crosslinked waterborne polyurethane-acrylic hybrids (WPU/AC-Ts) with a fixed acrylic monomer content (20 wt.%) and different trimethylol propane (TMP)/ethylene diamine (EDA) (0/0.20, 0.02/0.17, 0.04/0.14, 0.06/0.11, 0.08/0.08, the number indicated the mole% of TMP/EDA) for footwear adhesive materials were successfully prepared in this study. The as-polymerized hybrid emulsion containing 0.10/0.05 mole% of TMP/EDA content was found to be unstable, indicating that near 0.10/0.05 mole% of TMP/EDA content was beyond the limit value of crosslinkable TMP component for self-emulsifing. This study examined the effect of mole% of TMP/EDA on the stability and viscosity of hybrid emulsions, the tensile properties and dynamic mechanical thermal properties of hybrid film samples, and the adhesive strengths of formulated adhesives for footwear at both dry and wet states. As TMP content increased, the tensile strength/modulus/storage modulus/hardness of WPU/A...
تدمد: 1568-5616
0169-4243
URL الوصول: https://explore.openaire.eu/search/publication?articleId=doi_________::8d6535a238a183b983ffe8b198649adb
https://doi.org/10.1080/01694243.2017.1285744
رقم الأكسشن: edsair.doi...........8d6535a238a183b983ffe8b198649adb
قاعدة البيانات: OpenAIRE