Early fragmentation of polyester urethane sheet neither causes persistent oxidative stress nor alters the outcome of normal tissue healing in rat skin

التفاصيل البيبلوغرافية
العنوان: Early fragmentation of polyester urethane sheet neither causes persistent oxidative stress nor alters the outcome of normal tissue healing in rat skin
المؤلفون: SANDRO M. SGROTT, RODRIGO D. NEVES, ARMANDO J. D’ACAMPORA, GERALDO J.S. BERNARDES, LUIZ BELMONTE, THIAGO C. MARTINS, FRANCIANE BOBINSKI, EDUARDO CARGNIN-FERREIRA, ANDREZA HOEPERS, CLARISSA M. COMIM, DANIEL F. MARTINS, ANNA P. PIOVEZAN
المصدر: Anais da Academia Brasileira de Ciências, Vol 90, Iss 2 suppl 1, Pp 2211-2222 (2018)
بيانات النشر: Academia Brasileira de Ciências, 2018.
سنة النشر: 2018
المجموعة: LCC:Science
مصطلحات موضوعية: Polyurethane, inflammation, cytokines, oxidative stress, Wistar rats, Science
الوصف: Abstract Silicone breast implant is associated with complications inherent to the surgical procedure. Prosthesis coating with polyurethane, however, commonly reduces the incidence of such complications. In this paper, the authors evaluated the inflammatory histomorphometric profile and oxidative damage associated to the implant of polyester urethane sheets. Forty-eight Wistar rats were divided into Sham or polyester urethane groups (n = 8/group) and underwent a polyester urethane implant in the dorsal skinfold. Tissue samples were collected on days seven, 30, and 90 after surgery and subjected to histomorphometric analysis and biochemical tests. Results were analyzed by one-way ANOVA (p ≤ 0.05). Peri-implant tissue samples exhibited characteristic inflammatory response associated with the biomaterial, with increased vascularization on day seven and augmented levels of IL1-b and TNF-a after 30 days. Peri-implant fibrocystic population was small on day seven, but increased considerably after 90 days. A rise in the carbonyl group levels of skin samples in the polyester urethane group was observed on day seven. Findings suggest that polyester urethane sheets undergo biodegradation at an early stage after implantation, followed by increased vascularity and microencapsulation of biomaterial fragments, without persistent oxidative damage. Fiber arrangement inside the collagen matrix results in a fibrotic scar because of polyester urethane degradation.
نوع الوثيقة: article
وصف الملف: electronic resource
اللغة: English
تدمد: 1678-2690
0001-3765
Relation: http://www.scielo.br/scielo.php?script=sci_arttext&pid=S0001-37652018000502211&lng=en&tlng=en; https://doaj.org/toc/1678-2690
DOI: 10.1590/0001-3765201820170676
URL الوصول: https://doaj.org/article/8fe4b9773e104202aff03a22940e4b19
رقم الأكسشن: edsdoj.8fe4b9773e104202aff03a22940e4b19
قاعدة البيانات: Directory of Open Access Journals
الوصف
تدمد:16782690
00013765
DOI:10.1590/0001-3765201820170676